@misc{prasad_hot_working_2008, author={Prasad, Y.V.R.K.,Rao, K.P.,Hort, N.,Kainer, K.U.}, title={Hot working parameters and mechanisms in as-cast Mg-3Sn-1Ca alloy}, year={2008}, howpublished = {journal article}, doi = {https://doi.org/10.1016/j.matlet.2008.06.035}, abstract = {The hot working characteristics of as-cast Mg–3Sn–1Ca alloy have been studied using processing-map technique and the kinetic rate equation. The map exhibited two domains; one in the lower strain rate range (0.0003–0.01 s− 1) and the other in the higher strain rate range (0.1–10 s− 1)—both falling in the same temperature range of 350–550 s− 1. Hot extrusion at 500 °C and a speed corresponding to an average strain rate of 3 s− 1 exhibited dynamically recrystallized microstructure. The estimated apparent activation energy values are higher than those for self-diffusion in pure magnesium suggesting that the large volume fraction of MgSnCa intermetallic particles causes significant back stress.}, note = {Online available at: \url{https://doi.org/10.1016/j.matlet.2008.06.035} (DOI). Prasad, Y.; Rao, K.; Hort, N.; Kainer, K.: Hot working parameters and mechanisms in as-cast Mg-3Sn-1Ca alloy. Materials Letters. 2008. vol. 62, no. 26, 4207-4209. DOI: 10.1016/j.matlet.2008.06.035}}